Velho HC, Machado PS, da Rosa LS, Prochnow C, Pisani-Proença J. Is the adhesive or mechanical behavior of glass ceramics influenced by the adhesive layer application after etching and silanization? : A literature review. Braz. J. Oral Sci. [Internet]. 2023 Aug. 1 [cited 2024 May 6];22(00):e239056. Available from: https://periodicos.sbu.unicamp.br/ojs/index.php/bjos/article/view/8669056

Abstract

Aim: This review investigated the effect of applying an adhesive after surface treatment of glass-ceramics on the bonding, mechanical or clinical behavior. Methods: Studies comparing the adhesive, mechanical or clinical behavior of glass-ceramics, with or without adhesive application after surface treatment, were included. Searches were performed in PubMed, Scopus, and Web of Sciences databases (January 2022), resulting in 15 included studies. Results: Regarding the evaluated outcomes, 13 studies assessed bond strength, 2 studies assessed biaxial flexural strength and 1 study assessed fatigue failure load, while no study evaluating clinical outcomes was included. It was possible to observe that the adhesive application after ceramic surface treatment was unfavorable or did not influence the evaluated outcomes. Conclusion: Most of the evidence available in the literature shows that the adhesive application after surface treatment does not improve the adhesive and mechanical behavior of glass-ceramics.

https://doi.org/10.20396/bjos.v22i00.8669056
PDF

References

Gracis S, Thompson VP, Ferencz JL, Silva NR, Bonfante EA. A new classification system for all-ceramic and ceramic-like restorative materials. Int J Prosthodont. 2015 May-Jun;28(3):227-35. doi: 10.11607/ijp.4244.

Ritzberger C, Apel E, Höland W, Peschke A, Rheinberger VM. Properties and clinical application of three types of dental glass-ceramics and ceramics for CAD-CAM technologies. Materials (Basel). 2010 Jun;3(6):3700-13. doi: 10.3390/ma3063700.

Montazerian M, Zanotto ED. Bioactive and inert dental glass-ceramics. J Biomed Mater Res A. 2017 Feb;105(2):619-39. doi: 10.1002/jbm.a.35923.

Valenti M, Valenti A. Retrospective survival analysis of 261 lithium disilicate crowns in a private general practice. Quintessence Int. 2009 Jul-Aug;40(7):573-9.

Brentel AS, Ozcan M, Valandro LF, Alarça LG, Amaral R, Bottino MA. Microtensile bond strength of a resin cement to feldpathic ceramic after different etching and silanization regimens in dry and aged conditions. Dent Mater. 2007 Nov;23(11):1323-31. doi: 10.1016/j.dental.2006.11.011.

Prochnow C, Venturini AB, Grasel R, Gundel A, Bottino MC, Valandro LF. Adhesion to a lithium disilicate glass ceramic etched with hydrofluoric acid at distinct concentrations. Braz Dent J. 2018 Sep-Oct;29(5):492-9. doi: 10.1590/0103-6440201802080.

Venturini AB, Prochnow C, Rambo D, Gundel A, Valandro LF. Effect of hydrofluoric acid concentration on resin adhesion to a feldspathic ceramic. J Adhes Dent. 2015 Aug;17(4):313-20. doi: 10.3290/j.jad.a34592.

Ozcan M, Vallittu PK. Effect of surface conditioning methods on the bond strength of luting cement to ceramics. Dent Mater. 2003 Dec;19(8):725-31. doi: 10.1016/s0109-5641(03)00019-8.

Kalavacharla VK, Lawson NC, Ramp LC, Burgess JO. Influence of etching protocol and silane treatment with a universal adhesive on lithium disilicate bond strength. Oper Dent. 2015 Jul-Aug;40(4):372-8. doi: 10.2341/14-116-L.

Venturini AB, Prochnow C, Pereira GKR, Werner A, Kleverlaan CJ, Valandro LF. The effect of hydrofluoric acid concentration on the fatigue failure load of adhesively cemented feldspathic ceramic discs. Dent Mater. 2018 Apr;34(4):667-75. doi: 10.1016/j.dental.2018.01.010.

Sundfeld Neto D, Naves LZ, Costa AR, Correr AB, Consani S, Borges GA, et al. The Effect of hydrofluoric acid concentration on the bond strength and morphology of the surface and interface of glass ceramics to a resin cement. Oper Dent. 2015 Sep-Oct;40(5):470-9. doi: 10.2341/14-133-L.

El Zohairy AA, De Gee AJ, Mohsen MM, Feilzer AJ. Microtensile bond strength testing of luting cements to prefabricated CAD/CAM ceramic and composite blocks. Dent Mater. 2003 Nov;19(7):575-83. doi: 10.1016/s0109-5641(02)00107-0.

Murillo-Gómez F, Rueggeberg FA, De Goes MF. Short- and long-term bond strength between resin cement and glass-ceramic using a silane-containing universal adhesive. Oper Dent. 2017 Sep/Oct;42(5):514-25. doi: 10.2341/16-211-L.

Naves LZ, Soares CJ, Moraes RR, Gonçalves LS, Sinhoreti MA, Correr-Sobrinho L. Surface/interface morphology and bond strength to glass ceramic etched for different periods. Oper Dent. 2010 Jul-Aug;35(4):420-7. doi: 10.2341/09-152-L.

Nogueira IO, Oliveira PFG, Magno MB, Ferreira DMTP, Maia LC, Rabello TB. Does the application of an adhesive layer improve the bond strength of etched and silanized glass-ceramics to resin-based materials? A systematic review and meta-analysis. J Prosthet Dent. 2021 Jan;125(1):56-64. doi: 10.1016/j.prosdent.2019.12.005.

Romanini-Junior JC, Kumagai RY, Ortega LF, Rodrigues JA, Cassoni A, Hirata R, et al. Adhesive/silane application effects on bond strength durability to a lithium disilicate ceramic. J Esthet Restor Dent. 2018 Jul;30(4):346-51. doi: 10.1111/jerd.12387.

Barbon FJ, Moraes RR, Isolan CP, Spazzin AO, Boscato N. Influence of inorganic filler content of resin luting agents and use of adhesive on the performance of bonded ceramic. J Prosthet Dent. 2019 Dec;122(6):566.e1-566.e11. doi: 10.1016/j.prosdent.2019.09.013.

El Zohairy AA, De Gee AJ, Hassan FM, Feilzer AJ. The effect of adhesives with various degrees of hydrophilicity on resin ceramic bond durability. Dent Mater. 2004 Oct;20(8):778-87. doi: 10.1016/j.dental.2003.05.010.

Peumans M, Hikita K, De Munck J, Van Landuyt K, Poitevin A, Lambrechts P, et al. Effects of ceramic surface treatments on the bond strength of an adhesive luting agent to CAD-CAM ceramic. J Dent. 2007 Apr;35(4):282-8. doi: 10.1016/j.jdent.2006.09.006.

Meng X, Yoshida K, Atsuta M. Microshear bond strength of resin bonding systems to machinable ceramic with different surface treatments. J Adhes Dent. 2008 Jun;10(3):189-96.

Passos SP, Valandro LF, Amaral R, Ozcan M, Bottino MA, Kimpara ET. Does adhesive resin application contribute to resin bond durability on etched and silanized feldspathic ceramic? J Adhes Dent. 2008 Dec;10(6):455-60

Lise DP, Perdigão J, Van Ende A, Zidan O, Lopes GC. Microshear bond strength of resin cements to lithium disilicate substrates as a function of surface preparation. Oper Dent. 2015 Sep-Oct;40(5):524-32. doi: 10.2341/14-240-L.

Elsayed A, Younes F, Lehmann F, Kern M. Tensile bond strength of so-called universal primers and universal multimode adhesives to zirconia and lithium disilicate ceramics. J Adhes Dent. 2017;19(3):221-8. doi: 10.3290/j.jad.a38436.

Ataol AS, Ergun G. Effects of surface treatments on repair bond strength of a new CAD/CAM ZLS glass ceramic and two different types of CAD/CAM ceramics. J Oral Sci. 2018;60(2):201-211. doi: 10.2334/josnusd.17-0109.

Chen B, Lu Z, Meng H, Chen Y, Yang L, Zhang H, et al. Effectiveness of pre-silanization in improving bond performance of universal adhesives or self-adhesive resin cements to silica-based ceramics: chemical and in vitro evidences. Dent Mater. 2019 Apr;35(4):543-53. doi: 10.1016/j.dental.2019.01.010.

Murillo-Gómez F, Wanderley RB, De Goes MF. Impact of silane-containing universal adhesive on the biaxial flexural strength of a resin cement/glass-ceramic system. Oper Dent. 2019 Mar/Apr;44(2):200-9. doi: 10.2341/17-356-L.

Tribst JPM, Monteiro JB, Venturini AB, Pereira GKR, Bottino MA, Melo RM, et al. Fatigue failure load of resin-bonded simplified lithium disilicate glass-ceramic restorations: effect of ceramic conditioning methods. J Adhes Dent. 2019;21(4):373-81. doi: 10.3290/j.jad.a43000.

Südbeck JM, Jacker-Guhr S, Lührs AK. Do different pretreatment methods influence the microtensile bond strength of composite cements to silicate ceramic? J Adhes Dent. 2021 Jul;23(4):335-345. doi: 10.3290/j.jad.b1650153.

Edelhoff D, Ozcan M. To what extent does the longevity of fixed dental prostheses depend on the function of the cement? Working Group 4 materials: cementation. Clin Oral Implants Res. 2007 Jun;18 Suppl 3:193-204. doi: 10.1111/j.1600-0501.2007.01442.x. Erratum in: Clin Oral Implants Res. 2008 Mar;19(3):326-8.

Lührs AK, De Munck J, Geurtsen W, Van Meerbeek B. Composite cements benefit from light-curing. Dent Mater. 2014 Mar;30(3):292-301. doi: 10.1016/j.dental.2013.11.012.

El-Damanhoury HM, Gaintantzopoulou MD. Self-etching ceramic primer versus hydrofluoric acid etching: Etching efficacy and bonding performance. J Prosthodont Res. 2018 Jan;62(1):75-83. doi: 10.1016/j.jpor.2017.06.002.

Meyer Filho A, Vieira LC, Araújo E, Monteiro Júnior S. Effect of different ceramic surface treatments on resin microtensile bond strength. J Prosthodont. 2004 Mar;13(1):28-35. doi: 10.1111/j.1532-849X.2004.04007.x.

Denry I, Holloway JA. Ceramics for dental applications: a review. Materials (Basel). 2010 Jan;3(1):351-68. doi: 10.3390/ma3010351.

Armstrong S, Breschi L, Özcan M, Pfefferkorn F, Ferrari M, Van Meerbeek B. Academy of Dental Materials guidance on in vitro testing of dental composite bonding effectiveness to dentin/enamel using micro-tensile bond strength (μTBS) approach. Dent Mater. 2017 Feb;33(2):133-43. doi: 10.1016/j.dental.2016.11.015.

Armstrong S, Geraldeli S, Maia R, Raposo LH, Soares CJ, Yamagawa J. Adhesion to tooth structure: a critical review of "micro" bond strength test methods. Dent Mater. 2010 Feb;26(2):e50-62. doi: 10.1016/j.dental.2009.11.155.

Tribst JPM, Monteiro JB, Venturini AB, Pereira GKR, Bottino MA, Melo RM, et al. Fatigue Failure Load of Resin-bonded Simplified Lithium Disilicate Glass-Ceramic Restorations: Effect of Ceramic Conditioning Methods. J Adhes Dent. 2019;21(4):373-81. doi: 10.3290/j.jad.a43000.

Cardenas A, Siqueira F, Rocha J, Szesz A, Anwar M, El-Askary F, et al. Influence of conditioning time of universal adhesives on adhesive properties and enamel-etching pattern. Oper Dent. 2016 Sep-Oct;41(5):481-90. doi: 10.2341/15-213-L.

Muñoz M, Luque-Martinez I, Malaquias P, Hass V, Reis A, Campanha N, et al. In vitro longevity of bonding properties of universal adhesives to dentin. Oper Dent. 2015 May-Jun;40(3):282-92. doi: 10.2341/14-055-L.

Tsuchiya K, Takamizawa T, Barkmeier WW, Tsubota K, Tsujimoto A, Berry TP, et al. Effect of a functional monomer (MDP) on the enamel bond durability of single-step self-etch adhesives. Eur J Oral Sci. 2016 Feb;124(1):96-102. doi: 10.1111/eos.12232.

Yoshida Y, Nagakane K, Fukuda R, Nakayama Y, Okazaki M, Shintani H, et al. Comparative study on adhesive performance of functional monomers. J Dent Res. 2004 Jun;83(6):454-8. doi: 10.1177/154405910408300604.

Cardenas AM, Siqueira F, Hass V, Malaquias P, Gutierrez MF, Reis A, et al. Effect of MDP-containing silane and adhesive used alone or in combination on the long-term bond strength and chemical interaction with lithium disilicate ceramics. J Adhes Dent. 2017;19(3):203-12. doi: 10.3290/j.jad.a38414.

Shafiei F, Dehghani Z, Jowkar Z. The influence of the operator’s experience on the microleakage of two universal adhesives. Clin Exp Dent Res. 2021 Dec;7(6):951-6. doi: 10.1002/cre2.458.

Scotti N, Comba A, Gambino A, Manzon E, Breschi L, Paolino D, et al. Influence of operator experience on non-carious cervical lesion restorations: clinical evaluation with different adhesive systems. Am J Dent. 2016 Feb;29(1):33-8.

Creative Commons License

This work is licensed under a Creative Commons Attribution 4.0 International License.

Copyright (c) 2022 Helder Callegaro Velho, Pablo Soares Machado, Lucas Saldanha da Rosa , Catina Prochnow, Jatyr Pisani-Proença

Downloads

Download data is not yet available.